Commercial Oxsilan, 3-aminopropyltriethoxysilane and sol-gel siloxane coatings were applied on AA6016 aluminium alloy before electrocoating. Standard filiform corrosion test demonstrated the pre-treatment role on the under-paint corrosion rate. All pre-treatments increase the coating adhesion in water electrolyte (EIS). Anodic undermining is the mechanism of the coatings de-adhesion (SKP). Electromotive force (difference in potentials of defect-surrounding interface) and interface ability to promote the chloride migration are rate-determining factors of the filiform corrosion. Contrary to other pre-treatments, the aminosiloxane decreases the interfacial potential, facilitates the chlorides migration and leads to anodic de-adhesion of large coated areas (Tof-SIMS and EDXS). © 2012 Elsevier Ltd.
Filiform corrosion of electrocoated aluminium alloy: Role of surface pretreatment
Fedel, Michele;Deflorian, Flavio;
2012-01-01
Abstract
Commercial Oxsilan, 3-aminopropyltriethoxysilane and sol-gel siloxane coatings were applied on AA6016 aluminium alloy before electrocoating. Standard filiform corrosion test demonstrated the pre-treatment role on the under-paint corrosion rate. All pre-treatments increase the coating adhesion in water electrolyte (EIS). Anodic undermining is the mechanism of the coatings de-adhesion (SKP). Electromotive force (difference in potentials of defect-surrounding interface) and interface ability to promote the chloride migration are rate-determining factors of the filiform corrosion. Contrary to other pre-treatments, the aminosiloxane decreases the interfacial potential, facilitates the chlorides migration and leads to anodic de-adhesion of large coated areas (Tof-SIMS and EDXS). © 2012 Elsevier Ltd.I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione