The polymer-to-ceramic transformation of a polysilazane/divinylbenzene aerogel leading to SiCN aerogel was studied. The pre-ceramic samples were obtained by crosslinking a commercially available polysilazane with divinylbenzene in a highly diluted solution. Wet gels were supercritically dried using CO2 to get the pre-ceramic aerogel. The weight change during pyrolysis in flowing argon was studied by thermogravimetric analysis (in-situ measurements) and by measuring the weight change on samples pyrolyzed in a tubular furnace after cooling down to room temperature (ex-situ measurements). The structural transformation was followed by infrared spectroscopy while the microstructural changes were studied by nitrogen adsorption analysis. Results point out that samples pyrolyzed at intermediate temperature, i.e., around 600-800°C, react with the laboratory atmosphere forming SiO bonds and SiOH moieties. This out-of-furnace oxidation leads to an uncontrolled increase of the oxygen content of the pyrolyzed ceramics and eventually reduces the microporosity of the samples and its stability.

Out-of-furnace oxidation of SiCN polymer-derived ceramic aerogel pyrolized at intermediate temperature (600-800°C)

Zera, Emanuele;Sorarù, Gian Domenico
2016-01-01

Abstract

The polymer-to-ceramic transformation of a polysilazane/divinylbenzene aerogel leading to SiCN aerogel was studied. The pre-ceramic samples were obtained by crosslinking a commercially available polysilazane with divinylbenzene in a highly diluted solution. Wet gels were supercritically dried using CO2 to get the pre-ceramic aerogel. The weight change during pyrolysis in flowing argon was studied by thermogravimetric analysis (in-situ measurements) and by measuring the weight change on samples pyrolyzed in a tubular furnace after cooling down to room temperature (ex-situ measurements). The structural transformation was followed by infrared spectroscopy while the microstructural changes were studied by nitrogen adsorption analysis. Results point out that samples pyrolyzed at intermediate temperature, i.e., around 600-800°C, react with the laboratory atmosphere forming SiO bonds and SiOH moieties. This out-of-furnace oxidation leads to an uncontrolled increase of the oxygen content of the pyrolyzed ceramics and eventually reduces the microporosity of the samples and its stability.
2016
3
Zera, Emanuele; Nickel, W.; Kaskel, S.; Sorarù, Gian Domenico
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11572/174292
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 39
  • ???jsp.display-item.citation.isi??? 37
  • OpenAlex 40
social impact