We apply an in situ approach, whereby a polymer is incorporated into copper and evolves within the metal into the ceramic phase, to create a dispersion of hard particles in a metal. All constituents for the ceramic phase are contained within the organic polymer. The temperature for this polymer to ceramic conversion lies in the 1073 K to 1273 K (800 C to 1000 C) range. The process produces a nanoscale dispersion of the ceramic, which leads to high microhardness that remains unaltered at temperatures up to 1223 K (950 C) (0.9T M). Apparently, the introduction of the ceramic phase leads to the retention of copper crystallite size of a few hundred nm, despite exposure to heat treatments at these very high temperatures. We call these materials polymer-derived metal-matrix composites. © 2013 The Minerals, Metals & Materials Society and ASM International.
A novel in situ method for producing a dispersion of a ceramic phase into copper that remains stable at 0.9T
Ischia, Gloria;Molinari, Alberto;
2013-01-01
Abstract
We apply an in situ approach, whereby a polymer is incorporated into copper and evolves within the metal into the ceramic phase, to create a dispersion of hard particles in a metal. All constituents for the ceramic phase are contained within the organic polymer. The temperature for this polymer to ceramic conversion lies in the 1073 K to 1273 K (800 C to 1000 C) range. The process produces a nanoscale dispersion of the ceramic, which leads to high microhardness that remains unaltered at temperatures up to 1223 K (950 C) (0.9T M). Apparently, the introduction of the ceramic phase leads to the retention of copper crystallite size of a few hundred nm, despite exposure to heat treatments at these very high temperatures. We call these materials polymer-derived metal-matrix composites. © 2013 The Minerals, Metals & Materials Society and ASM International.I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione