In this paper a set of specimens, used for the critical distance determination, are investigated with a non-contact 3D optical profiler. The fatigue fracture surfaces of both plain and V-notched specimens, under axial (mode I) and torsional (mode III) loadings are observed, investigating steel 42CrMo4+QT and aluminium alloy 7075-T6. The fatigue fracture profiles are compared to be previously obtained critical distances, both for mode I and mode III. The stage I to stage II transition was found at a smaller size than the axial critical distance, for the steel, while for the torsional load a local plateau at the nucleation was observed. The fracture surface of the axial loading was instead much irregular at the scale of the mode I critical distance, for the aluminium alloy, resembling a not concluded stage I, while again a relatively flat surface was observed for the mode III loading.

Fatigue fracture surface investigations with a 3D optical profiler / Santus, C.; Neri, P.; Romoli, L.; Lutey, A.; Raghavendra, S.; Benedetti, M.. - In: PROCEDIA STRUCTURAL INTEGRITY. - ISSN 2452-3216. - ELETTRONICO. - 39:(2022), pp. 450-459. [10.1016/j.prostr.2022.03.114]

Fatigue fracture surface investigations with a 3D optical profiler

Raghavendra, S.;Benedetti, M.
2022-01-01

Abstract

In this paper a set of specimens, used for the critical distance determination, are investigated with a non-contact 3D optical profiler. The fatigue fracture surfaces of both plain and V-notched specimens, under axial (mode I) and torsional (mode III) loadings are observed, investigating steel 42CrMo4+QT and aluminium alloy 7075-T6. The fatigue fracture profiles are compared to be previously obtained critical distances, both for mode I and mode III. The stage I to stage II transition was found at a smaller size than the axial critical distance, for the steel, while for the torsional load a local plateau at the nucleation was observed. The fracture surface of the axial loading was instead much irregular at the scale of the mode I critical distance, for the aluminium alloy, resembling a not concluded stage I, while again a relatively flat surface was observed for the mode III loading.
2022
Santus, C.; Neri, P.; Romoli, L.; Lutey, A.; Raghavendra, S.; Benedetti, M.
Fatigue fracture surface investigations with a 3D optical profiler / Santus, C.; Neri, P.; Romoli, L.; Lutey, A.; Raghavendra, S.; Benedetti, M.. - In: PROCEDIA STRUCTURAL INTEGRITY. - ISSN 2452-3216. - ELETTRONICO. - 39:(2022), pp. 450-459. [10.1016/j.prostr.2022.03.114]
File in questo prodotto:
File Dimensione Formato  
1-s2.0-S2452321622003274-main.pdf

accesso aperto

Tipologia: Versione editoriale (Publisher’s layout)
Licenza: Creative commons
Dimensione 2.65 MB
Formato Adobe PDF
2.65 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11572/337718
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 2
  • ???jsp.display-item.citation.isi??? ND
social impact